Peripheral surface spraying process points

2023-01-06 14:14:18

And the shaft part of the same spraying, the coating shrinkage force so that the coating tighten the matrix, is conducive to the binding strength of the Bureau, the pit body heat temperature to take the lower limit, spraying process, the workpiece temperature to more than 250 ℃, must also explain the shape,And spray parts of different parts of the workpiece temperature control should also have different requirements, when spraying small parts of the cylindrical parts, avoid the workpiece temperature is too high, cooling, the workpiece shrinkage stress, will lead to the coating off or cause a larger Deformation.